Beilstein J. Nanotechnol. 2015, 6, 1897–1903, doi:10.3762/bjnano.6.193
Figure 1: TEM images of pristine ZnO (a) and TiO2 (b) NPs.
Figure 2: FTIR spectra of untreated and hydroxylated ZnO NPs.
Figure 3: FTIR spectra of untreated and hydroxylated TiO2 NPs.
Figure 4: TEM images of H2O2-treated ZnO NPs (a) and XRD spectra before and after H2O2 treatment (b).
Figure 5: Temperature-dependent size change of H2O2-treated TiO2 NPs (a), untreated TiO2 NPs (b) and the size...
Figure 6: Temperature-dependent size change of H2O2-treated ZnO NPs (a), untreated ZnO NPs (b) and the change...